{"id":154,"date":"2025-04-30T01:31:34","date_gmt":"2025-04-30T01:31:34","guid":{"rendered":"https:\/\/www.syringetest.com\/?page_id=154"},"modified":"2026-05-09T06:36:31","modified_gmt":"2026-05-09T06:36:31","slug":"finger-flange-breakage-force-test","status":"publish","type":"page","link":"https:\/\/www.syringetest.com\/id\/finger-flange-breakage-force-test","title":{"rendered":"Uji Kekuatan Kerusakan Flensa Jari"},"content":{"rendered":"<div data-elementor-type=\"wp-page\" data-elementor-id=\"154\" class=\"elementor elementor-154\" data-elementor-post-type=\"page\">\n\t\t\t\t<div class=\"elementor-element elementor-element-247db7c e-flex e-con-boxed e-con e-parent\" data-id=\"247db7c\" data-element_type=\"container\" data-e-type=\"container\" data-settings=\"{&quot;background_background&quot;:&quot;classic&quot;}\">\n\t\t\t\t\t<div class=\"e-con-inner\">\n\t\t\t\t<div class=\"elementor-element elementor-element-ab06118 elementor-widget elementor-widget-heading\" data-id=\"ab06118\" data-element_type=\"widget\" data-e-type=\"widget\" data-widget_type=\"heading.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t<h1 class=\"elementor-heading-title elementor-size-default\">Pengujian Kekuatan Kerusakan Flensa Jari<\/h1>\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<div class=\"elementor-element elementor-element-62cf733 elementor-widget elementor-widget-text-editor\" data-id=\"62cf733\" data-element_type=\"widget\" data-e-type=\"widget\" data-widget_type=\"text-editor.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t\t\t\t\t<p>Dalam industri kemasan farmasi dan medis, <strong>kekuatan kerusakan flensa jari<\/strong> adalah indikator kinerja penting untuk memastikan keandalan struktural laras jarum suntik. Parameter ini, didefinisikan dan distandarisasi dalam <strong><em><a href=\"https:\/\/www.syringetest.com\/id\/standards\/iso-11040-4\/\">ISO 11040-4<\/a> Lampiran C1<\/em><\/strong>membantu produsen dan profesional jaminan kualitas menilai apakah flensa jarum suntik dapat menahan tekanan mekanis selama penanganan dan injeksi.<\/p><p>Memahami pengukuran ini dan metode pengujian standarnya sangat penting bagi para profesional yang terlibat dalam <strong>pengujian jarum suntik<\/strong>terutama untuk jarum suntik sub-rakitan steril yang ditujukan untuk larutan injeksi.<\/p>\t\t\t\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t<div class=\"elementor-element elementor-element-3f136d2 e-flex e-con-boxed e-con e-parent\" data-id=\"3f136d2\" data-element_type=\"container\" data-e-type=\"container\" data-settings=\"{&quot;background_background&quot;:&quot;classic&quot;}\">\n\t\t\t\t\t<div class=\"e-con-inner\">\n\t\t\t\t<div class=\"elementor-element elementor-element-b673494 elementor-widget elementor-widget-heading\" data-id=\"b673494\" data-element_type=\"widget\" data-e-type=\"widget\" data-widget_type=\"heading.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t<h2 class=\"elementor-heading-title elementor-size-default\">Pentingnya Gaya Patah Flensa Jari dalam Integritas Jarum Suntik<\/h2>\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<div class=\"elementor-element elementor-element-aa819a0 elementor-widget elementor-widget-text-editor\" data-id=\"aa819a0\" data-element_type=\"widget\" data-e-type=\"widget\" data-widget_type=\"text-editor.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t\t\t\t\t<p>The <strong>kekuatan kerusakan flensa jari<\/strong> mengacu pada gaya mekanis maksimum yang dapat ditahan oleh flensa jarum suntik sebelum mengalami kegagalan. Nilai ini menunjukkan ketahanan jarum suntik, terutama ketika pengguna memberikan tekanan selama injeksi atau ketika sistem pengisian otomatis mencengkeram jarum suntik.<\/p><p>Kekuatan patah yang tidak memadai dapat menyebabkan keretakan flensa atau kegagalan total, sehingga menimbulkan bahaya keselamatan. Oleh karena itu, menjaga kualitas yang konsisten di seluruh batch tidak dapat dinegosiasikan dalam pembuatan perangkat medis.<\/p>\t\t\t\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t<div class=\"elementor-element elementor-element-37feff9 e-flex e-con-boxed e-con e-parent\" data-id=\"37feff9\" data-element_type=\"container\" data-e-type=\"container\" data-settings=\"{&quot;background_background&quot;:&quot;classic&quot;}\">\n\t\t\t\t\t<div class=\"e-con-inner\">\n\t\t\t\t<div class=\"elementor-element elementor-element-3146496 elementor-widget elementor-widget-heading\" data-id=\"3146496\" data-element_type=\"widget\" data-e-type=\"widget\" data-widget_type=\"heading.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t<h2 class=\"elementor-heading-title elementor-size-default\">Uji Gaya Kerusakan Flensa Jari - ISO 11040-4 Lampiran C1<\/h2>\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<div class=\"elementor-element elementor-element-08fc359 elementor-widget elementor-widget-text-editor\" data-id=\"08fc359\" data-element_type=\"widget\" data-e-type=\"widget\" data-widget_type=\"text-editor.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t\t\t\t\t<p>The <strong><a href=\"https:\/\/www.syringetest.com\/id\/standards\/iso-11040-4\/\" target=\"_blank\" rel=\"noopener\" data-wplink-edit=\"true\">ISO 11040-4<\/a> Lampiran C1<\/strong> menguraikan metode pengujian untuk mengevaluasi ketahanan kerusakan flensa. Prosedur ini memastikan hasil yang akurat dan dapat diulang, sehingga menjadikannya standar emas dalam pengujian kinerja jarum suntik.<\/p>\t\t\t\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t<div class=\"elementor-element elementor-element-fd10895 e-grid e-con-full e-con e-child\" data-id=\"fd10895\" data-element_type=\"container\" data-e-type=\"container\">\n\t\t\t\t<div class=\"elementor-element elementor-element-d98b842 elementor-widget elementor-widget-text-editor\" data-id=\"d98b842\" data-element_type=\"widget\" data-e-type=\"widget\" data-widget_type=\"text-editor.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t\t\t\t\t<h3>Tujuan Tes<\/h3><p>Untuk menentukan ketahanan kerusakan flensa dengan menerapkan gaya ke bawah pada laras jarum suntik dengan menggunakan peralatan khusus. Tes ini mengevaluasi kedua <strong>kekuatan barel kaca<\/strong> dan kompatibilitasnya dengan desain jarum suntik lainnya.<\/p>\t\t\t\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<div class=\"elementor-element elementor-element-db58dbc elementor-widget elementor-widget-text-editor\" data-id=\"db58dbc\" data-element_type=\"widget\" data-e-type=\"widget\" data-widget_type=\"text-editor.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t\t\t\t\t<h3>Peralatan yang Diperlukan<\/h3><ul><li><strong>Mesin uji tarik dan kompresi universal<\/strong>: Harus menyertakan sel beban yang sesuai dan kecepatan uji yang dapat dikonfigurasi <strong>100 mm\/menit<\/strong>.<\/li><li><strong>Tempat jarum suntik<\/strong>: Biasanya dibuat dari bahan PEEK, disesuaikan dengan dimensi jarum suntik.<\/li><li><strong>Memuat pin<\/strong>: Terbuat dari poliasetale atau baja tahan karat, didesain untuk menerapkan gaya secara seragam.<\/li><\/ul>\t\t\t\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<div class=\"elementor-element elementor-element-a8c15d0 elementor-widget elementor-widget-image\" data-id=\"a8c15d0\" data-element_type=\"widget\" data-e-type=\"widget\" data-widget_type=\"image.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t\t\t\t\t\t\t\t\t\t\t<img fetchpriority=\"high\" decoding=\"async\" width=\"800\" height=\"202\" src=\"https:\/\/www.syringetest.com\/wp-content\/uploads\/2025\/04\/Syringe-Finger-Flange-Breakage-Force-Test-ISO-11040-4-Annex-C1-1024x258.webp\" class=\"attachment-large size-large wp-image-163\" alt=\"Uji Gaya Kerusakan Flensa Jari Jarum Suntik - ISO 11040-4 Lampiran C1\" srcset=\"https:\/\/www.syringetest.com\/wp-content\/uploads\/2025\/04\/Syringe-Finger-Flange-Breakage-Force-Test-ISO-11040-4-Annex-C1-1024x258.webp 1024w, https:\/\/www.syringetest.com\/wp-content\/uploads\/2025\/04\/Syringe-Finger-Flange-Breakage-Force-Test-ISO-11040-4-Annex-C1-300x76.webp 300w, https:\/\/www.syringetest.com\/wp-content\/uploads\/2025\/04\/Syringe-Finger-Flange-Breakage-Force-Test-ISO-11040-4-Annex-C1-768x194.webp 768w, https:\/\/www.syringetest.com\/wp-content\/uploads\/2025\/04\/Syringe-Finger-Flange-Breakage-Force-Test-ISO-11040-4-Annex-C1.webp 1190w\" sizes=\"(max-width: 800px) 100vw, 800px\" \/>\t\t\t\t\t\t\t\t\t\t\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t<div class=\"elementor-element elementor-element-3a78210 e-flex e-con-boxed e-con e-parent\" data-id=\"3a78210\" data-element_type=\"container\" data-e-type=\"container\" data-settings=\"{&quot;background_background&quot;:&quot;classic&quot;}\">\n\t\t\t\t\t<div class=\"e-con-inner\">\n\t\t\t\t<div class=\"elementor-element elementor-element-e89a55d elementor-widget elementor-widget-heading\" data-id=\"e89a55d\" data-element_type=\"widget\" data-e-type=\"widget\" data-widget_type=\"heading.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t<h2 class=\"elementor-heading-title elementor-size-default\">Pengaturan dan Eksekusi Pengujian Jarum Suntik<\/h2>\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<div class=\"elementor-element elementor-element-2e8f3f2 elementor-widget elementor-widget-text-editor\" data-id=\"2e8f3f2\" data-element_type=\"widget\" data-e-type=\"widget\" data-widget_type=\"text-editor.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t\t\t\t\t<p>Untuk melakukan pengujian seperti yang ditentukan dalam <strong>Pengujian ISO 11040-4<\/strong>ikuti langkah-langkah berikut ini:<\/p><h3>1. Persiapan Sampel<\/h3><p>Hindari guncangan atau kesalahan penanganan laras jarum suntik sebelum melakukan pengujian. Periksa dudukan dan pin apakah ada keausan.<\/p><h3>2. Pengaturan Peralatan<\/h3><ul><li>Tempatkan jarum suntik pada dudukan di bawah flensa.<\/li><li>Sejajarkan pin pemuatan untuk menerapkan gaya pada kedalaman flensa laras.<\/li><\/ul><h3>3. Eksekusi Tes<\/h3><ul><li>Jalankan mesin pada <strong>100 mm\/menit<\/strong>.<\/li><li>Catat grafik perpindahan gaya.<\/li><li>Gunakan <strong>laju pengambilan sampel minimal 500 Hz<\/strong> untuk deteksi gaya puncak.<\/li><\/ul><h3>4. Analisis Hasil<\/h3><p>Gaya puncak yang diamati sebelum kegagalan flensa dicatat sebagai <strong>kekuatan kerusakan flensa jari<\/strong>. ISO 11040-4 Lampiran C1 menetapkan bahwa nilai ini, bersama dengan kecepatan uji dan jumlah sampel, harus dilaporkan dalam dokumentasi akhir.<\/p>\t\t\t\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t<div class=\"elementor-element elementor-element-2d148ee e-grid e-con-full e-con e-parent\" data-id=\"2d148ee\" data-element_type=\"container\" data-e-type=\"container\" data-settings=\"{&quot;background_background&quot;:&quot;classic&quot;}\">\n\t\t\t\t<div class=\"elementor-element elementor-element-ef5e9b3 elementor-widget elementor-widget-image\" data-id=\"ef5e9b3\" data-element_type=\"widget\" data-e-type=\"widget\" data-widget_type=\"image.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t\t\t\t\t\t\t\t\t\t\t<img decoding=\"async\" width=\"800\" height=\"643\" src=\"https:\/\/www.syringetest.com\/wp-content\/uploads\/2025\/04\/06a8c2a0-image-3.png\" class=\"attachment-large size-large wp-image-65\" alt=\"\" srcset=\"https:\/\/www.syringetest.com\/wp-content\/uploads\/2025\/04\/06a8c2a0-image-3.png 875w, https:\/\/www.syringetest.com\/wp-content\/uploads\/2025\/04\/06a8c2a0-image-3-300x241.png 300w, https:\/\/www.syringetest.com\/wp-content\/uploads\/2025\/04\/06a8c2a0-image-3-768x617.png 768w\" sizes=\"(max-width: 800px) 100vw, 800px\" \/>\t\t\t\t\t\t\t\t\t\t\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t<div class=\"elementor-element elementor-element-f83c119 e-con-full e-flex e-con e-child\" data-id=\"f83c119\" data-element_type=\"container\" data-e-type=\"container\">\n\t\t\t\t<div class=\"elementor-element elementor-element-af86f15 elementor-widget elementor-widget-heading\" data-id=\"af86f15\" data-element_type=\"widget\" data-e-type=\"widget\" data-widget_type=\"heading.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t<h2 class=\"elementor-heading-title elementor-size-default\">Mengapa Memilih <b>Syringetest.com?<\/b><\/h2>\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<div class=\"elementor-element elementor-element-321653d elementor-widget elementor-widget-text-editor\" data-id=\"321653d\" data-element_type=\"widget\" data-e-type=\"widget\" data-widget_type=\"text-editor.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t\t\t\t\t<p>Pengujian gaya kerusakan flensa yang akurat membutuhkan instrumen berkinerja tinggi. Di <strong>Syringetest.com<\/strong>kami menawarkan penguji tarik dan kompresi canggih yang disesuaikan untuk <strong>pengujian jarum suntik<\/strong>sepenuhnya sesuai dengan <a href=\"https:\/\/www.iso.org\/standard\/82222.html\" target=\"_blank\" rel=\"noopener\"><em>ISO 11040-4<\/em><\/a>. Sistem kami dilengkapi dengan sel beban yang presisi, kecepatan yang dapat disesuaikan, dan perangkat lunak yang intuitif untuk visualisasi dan ekspor data secara real-time.<\/p><p>Kami juga menawarkan <strong>tempat jarum suntik khusus dan integrasi otomatisasi<\/strong>membantu merampingkan pengujian dalam lingkungan produksi dengan throughput tinggi.<\/p>\t\t\t\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<div class=\"elementor-element elementor-element-262c330 elementor-widget__width-auto elementor-align-left elementor-widget elementor-widget-button\" data-id=\"262c330\" data-element_type=\"widget\" data-e-type=\"widget\" data-widget_type=\"button.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t\t\t\t\t<div class=\"elementor-button-wrapper\">\n\t\t\t\t\t<a class=\"elementor-button elementor-button-link elementor-size-sm\" href=\"https:\/\/www.syringetest.com\/id\/contact-us\/\">\n\t\t\t\t\t\t<span class=\"elementor-button-content-wrapper\">\n\t\t\t\t\t\t\t\t\t<span class=\"elementor-button-text\">Hubungi Kami<\/span>\n\t\t\t\t\t<\/span>\n\t\t\t\t\t<\/a>\n\t\t\t\t<\/div>\n\t\t\t\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<\/div>","protected":false},"excerpt":{"rendered":"<p>Finger Flange Breakage Force Testing In the pharmaceutical and medical packaging industry, finger flange breakage force is a critical performance indicator for ensuring the structural reliability of syringe barrels. This parameter, defined and standardized in ISO 11040-4 Annex C1, helps manufacturers and quality assurance professionals assess whether the syringe flange can withstand mechanical stress during [&hellip;]<\/p>\n","protected":false},"author":2,"featured_media":0,"parent":0,"menu_order":0,"comment_status":"closed","ping_status":"closed","template":"elementor_header_footer","meta":{"footnotes":""},"class_list":["post-154","page","type-page","status-publish","hentry"],"_links":{"self":[{"href":"https:\/\/www.syringetest.com\/id\/wp-json\/wp\/v2\/pages\/154","targetHints":{"allow":["GET"]}}],"collection":[{"href":"https:\/\/www.syringetest.com\/id\/wp-json\/wp\/v2\/pages"}],"about":[{"href":"https:\/\/www.syringetest.com\/id\/wp-json\/wp\/v2\/types\/page"}],"author":[{"embeddable":true,"href":"https:\/\/www.syringetest.com\/id\/wp-json\/wp\/v2\/users\/2"}],"replies":[{"embeddable":true,"href":"https:\/\/www.syringetest.com\/id\/wp-json\/wp\/v2\/comments?post=154"}],"version-history":[{"count":0,"href":"https:\/\/www.syringetest.com\/id\/wp-json\/wp\/v2\/pages\/154\/revisions"}],"wp:attachment":[{"href":"https:\/\/www.syringetest.com\/id\/wp-json\/wp\/v2\/media?parent=154"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}